Jump to content

Thermowood

From RUVARO Sauna Wiki

Thermowood commonly refers to ThermoWood®, a registered trade mark applied to timber made by licensed producers using a Finnish heat-and-steam thermal-modification system. It is neither a wood species nor the generic term for all thermally modified timber. Source species, product class, grade and intended application remain part of a ThermoWood® product's identity.

Thermal modification alters wood chemistry as well as moisture response, colour and mechanical behaviour. The outcome depends on species and process conditions, so the mark does not make every product suitable for a sauna wall, seat or exterior. In the branded process, “no added chemical reagent” describes process inputs; it does not mean chemically unchanged or emission-free wood.

Trade mark and technical terminology

A 2024 WIPO administrative decision records European Union trade mark no. 000922765, filed in 1998 and registered in 2000 for building materials, and identifies Lämpöpuuyhdistys Ry, the Finnish association operating as the International ThermoWood Association, as proprietor.[1] The decision establishes the recorded rights and dates, not technical performance.

The association attributes industrial development to VTT Technical Research Centre of Finland and participating wood companies. It states that the association was founded in 2000 and received a licence to the mark in 2001.[2] This is the rights holder's history, not an independent account or evidence for a single inventor. Trade-mark rights should not be conflated with the lifecycle of patents.

In contrast, DD CEN/TS 15679 uses “thermally modified timber” generically for a semi-finished material whose relevant characteristics depend on end use.[3] BSI listed this British adoption as current and under review on 5 September 2026. The technical specification grants neither use of the mark nor approval for a Sauna.

Process and classes

The association's 2025 handbook divides manufacture into high-temperature drying, thermal modification, and cooling with moisture conditioning. It describes heat, steam and water at atmospheric pressure without an added chemical reagent; the minimum modification temperature is 160 °C and the stated moisture content after cooling is 4–7%.[4] Those specifications define the branded system rather than every thermal-treatment kiln.

Three equal panels linked left to right: high-temperature drying, thermal modification, then cooling and conditioning, with a note on protective steam.
Schematic sequence of the ThermoWood manufacturing process. Operating settings depend on the wood species, product class and material dimensions; this is not a kiln operating recipe.

The product classes are Thermo-S, for stability, and Thermo-D, for durability. Conditions remain species-specific. The handbook lists Nordic pine and spruce at 190 °C (±3 °C) for Thermo-S and 212 °C (±3 °C) for Thermo-D; radiata-pine Thermo-D is listed at 230 °C (±3 °C).[4] These set-points do not transfer to another species, process or unlicensed product.

Association auditing and licensed production provide process oversight. They do not replace botanical identification, construction-product declarations or forest chain of custody. A darkened board without records is not demonstrated to be ThermoWood®, and its colour cannot identify a class or modification intensity.

Property changes and their limits

Heat degrades and rearranges wood constituents, especially hemicelluloses, and forms volatile and non-volatile products. Hill, Altgen and Rautkari review commercial thermal-modification processes commonly operating at about 160–240 °C while differing in moisture, atmosphere, pressure, time and temperature.[5] This scientific range describes a broader field; it is not the Thermo-S and Thermo-D class table.

Modification commonly reduces equilibrium moisture content and can improve dimensional stability compared with untreated controls, but it does not stop hygroscopic exchange. Hill and colleagues report partial reversal of reduced hygroscopicity after high-humidity or liquid-water exposure in some dry-process studies, and differences between wet and dry processes at comparable mass loss.[5] Calling the timber waterproof misstates the mechanism and evidence.

Decay resistance can increase with treatment intensity, but species, process control and test method affect the result. Candelier and colleagues found that individual process-control proxies have limits and that the properties conferred on the product require suitable quality assessment.[6] Dark colour is not a durability certificate, while resistance to selected fungi does not imply resistance to every mould, insect or persistently wet condition.

Benefits are accompanied by trade-offs. Thermal modification causes mass loss and can reduce bending, splitting, impact or fracture performance. Aytin, Çakıcıer and Birtürk found lower shrinkage and swelling but species-dependent chemical and mechanical outcomes in four Turkish-grown species treated by the ThermoWood® method at 212 °C for one hour.[7] Their material tests cannot establish the capacity of a full-size sauna assembly.

The current handbook states that ThermoWood® is not available as strength-graded timber and must not be used for load-bearing structures.[4] A favourable result from one material test cannot override that system restriction. Load-bearing supports beneath a seat or lining therefore require a separately verified construction.

Sauna applications

Association documentation illustrates ThermoWood® wall, ceiling and sauna-bench products.[2] This demonstrates intended applications, not blanket approval. Interior lining, seating and external cladding differ in load, contact, wetting, ultraviolet exposure and repair access.

BS EN 14915 includes thermally modified solid-wood panelling and cladding within its defined product scope.[8] It is not a bench or structural standard. Product form, thickness, profile, declared properties, mounting and substrate must still match the evidence used in Sauna construction.

Source wood remains part of the description. The articles on alder, abachi and hemlock separate untreated properties from bounded modification studies; cedar illustrates why a trade name may not even identify a species. The mark neither erases these distinctions nor ranks the species.

Within a Sauna room, joints, fixings, cavities, water paths and cleaning are assembly questions. The handbook does not recommend the product for direct soil or water contact and notes that superficial mould can still occur.[4] Lower equilibrium moisture does not remove drainage and drying requirements; ultraviolet greying outdoors is also different from hot-room ageing.

Contact, emissions and fire

Lower bulk thermal conductivity is sometimes turned into a claim of touch safety. ISO 13732-1 instead assesses responses to hot-solid contact using material and contact duration among the conditions; it gives no universal safe surface temperature and does not address discomfort.[9] Actual surface temperature, geometry, finish, moisture and exposed metal remain relevant.

Outline of a sauna interior with six source markers, including solid timber, a marked heat-treated board, surface finishes, cleaning products, fragrance over the heater and a wood stove with flue, each linked to a box naming compound groups such as terpenes, aldehydes and organic acids.
Sources of volatile organic compounds in a sauna. Heat-treated timber has a changed emission profile rather than none, while finishes, cleaning products, fragrance on hot stones and any escaping combustion gases are separate sources. No concentrations are implied. Schematic.

Modification changes volatile-organic-compound profiles rather than eliminating emissions. A 2019 review found species- and treatment-dependent patterns: total VOCs generally fell in the treated-softwood studies it surveyed but rose for treated hardwoods, while compound composition changed.[10] A six-species headspace experiment likewise reported reductions and increases among individual compounds depending on process and species.[11] Neither measured an installed-sauna dose or clinical risk; “VOC-free”, “non-toxic” and “therapeutic odour” exceed the evidence.

The mark supplies no reaction-to-fire class. BS EN 13501-1 bases classification on test results for a construction product in an end-use arrangement.[12] Species, product class, thickness, mounting and substrate must match the declaration; modification alone establishes neither fire resistance nor heater clearance.

Installation and sourcing

The association handbook links lower pH after modification to possible corrosion and specifies at least A2 stainless steel for sauna wall and ceiling cladding and benches.[4] Product and project documentation still govern fastener dimensions and geometry. Increased brittleness and fine dry machining dust can also require adjusted tools and handling.

UK Health and Safety Executive guidance calls for source extraction, dust-free cleaning and suitable respiratory protection where further control is needed for wood dust.[13] Those workplace controls concern cutting and sanding, not normal contact with an intact installed surface.

FSC chain of custody tracks eligible forest-based material through a supply chain but certifies neither sauna performance, emissions nor a comparative carbon result.[14] FSC-certified sauna wood, PEFC-certified sauna wood, Sustainable sauna wood and local sourcing are separate from process licensing. Environmental comparison needs a declared product, geography, service life, maintenance and end-of-life scenario rather than the mark alone.

A complete schedule records the licensed producer, current product document, source species, Thermo-S or Thermo-D class, grade, dimensions, component, supports, fasteners, finish, contact and fire evidence, cleaning regime and provenance. This gives Sauna design a defined product instead of treating ThermoWood® as a universal upgrade.

References

  1. ↑ World Intellectual Property Organization Arbitration and Mediation Center, Lämpöpuuyhdistys Ry v. Privacy Protect, LLC / Global Forest Lumber Company LLC, Blue Lake Lumber LLC, Case No. D2023-4796, 2024, https://www.wipo.int/amc/en/domains/decisions/pdf/2023/d2023-4796.pdf, accessed 5 September 2026.
  2. ↑ 2.0 2.1 International ThermoWood Association, “ThermoWood®”, https://thermowood.com/thermowood, accessed 5 September 2026.
  3. ↑ British Standards Institution, DD CEN/TS 15679:2007, Thermal modified timber — Definitions and characteristics, published 29 February 2008, current and under review, https://knowledge.bsigroup.com/products/thermal-modified-timber-definitions-and-characteristics, accessed 5 September 2026.
  4. ↑ 4.0 4.1 4.2 4.3 4.4 International ThermoWood Association, ThermoWood® Handbook 2025, second updated release, Helsinki/Lahti, October 2025, 68 pp., https://thermowood.fi/dataflow/thermowood/files/media/thermowood_handbook_2025_web_17.pdf, accessed 5 September 2026.
  5. ↑ 5.0 5.1 Callum Hill, Michael Altgen and Lauri Rautkari, “Thermal modification of wood—a review: chemical changes and hygroscopicity”, Journal of Materials Science, volume 56, 2021, pp. 6581–6614. doi:10.1007/s10853-020-05722-z.
  6. ↑ Kévin Candelier, Marie-France Thevenon, Anélie Petrissans, Stéphane Dumarcay, Philippe Gérardin and Mathieu Pétrissans, “Control of wood thermal treatment and its effects on decay resistance: a review”, Annals of Forest Science, volume 73, 2016, pp. 571–583. doi:10.1007/s13595-016-0541-x.
  7. ↑ Ayhan Aytin, Nevzat Çakıcıer and Turgay Birtürk, “Chemical, hygroscopic, and mechanical properties of various wood species heat treated via the ThermoWood® method”, BioResources, volume 17, issue 1, 2022, pp. 785–801. doi:10.15376/biores.17.1.785-801.
  8. ↑ British Standards Institution, BS EN 14915:2013+A2:2020, Solid wood panelling and cladding — Characteristics, requirements and marking, published 30 June 2020, https://knowledge.bsigroup.com/products/solid-wood-panelling-and-cladding-characteristics-requirements-and-marking, accessed 5 September 2026.
  9. ↑ International Organization for Standardization, ISO 13732-1:2006, Ergonomics of the thermal environment — Methods for the assessment of human responses to contact with surfaces — Part 1: Hot surfaces, confirmed 2022, https://www.iso.org/standard/43558.html, accessed 5 September 2026.
  10. ↑ Jure Pohleven, Michael D. Burnard and Andreja Kutnar, “Volatile organic compounds emitted from untreated and thermally modified wood — a review”, Wood and Fiber Science, volume 51, issue 3, 2019, pp. 231–254. doi:10.22382/wfs-2019-023.
  11. ↑ Andrea Romano, Luca Cappellin, Ignazia Cuccui, Sara Bogialli, Iuliia Khomenko, Matteo Tonezzer, Franco Biasioli, Paolo Pastore and Ottaviano Allegretti, “Exploring volatile organic compound emission from thermally modified wood by PTR-ToF-MS”, Analyst, volume 147, issue 22, 2022, pp. 5138–5148. doi:10.1039/D2AN01376B.
  12. ↑ British Standards Institution, BS EN 13501-1:2018, Fire classification of construction products and building elements — Classification using data from reaction to fire tests, published 31 January 2019, https://knowledge.bsigroup.com/products/fire-classification-of-construction-products-and-building-elements-classification-using-data-from-reaction-to-fire-tests, accessed 5 September 2026.
  13. ↑ UK Health and Safety Executive, “Wood dust”, updated 4 September 2025, https://www.hse.gov.uk/woodworking/wooddust.htm, accessed 5 September 2026.
  14. ↑ Forest Stewardship Council, “Chain of Custody Certification”, https://fsc.org/en/chain-of-custody, accessed 5 September 2026.

Template:Sauna construction